1, deformation ------ products do not meet the requirements of the design of the shape.
2, the mouth and ear crooked ------ refers to the mouth, ears, the height discomfort, crooked.
3, pimple ------ underglaze billet body convex nodular solid body.
4. Blank bubble ------ Hollow bubble raised under glaze body.
5. Mud residue ------ The defects caused by the mud debris and glaze residue remaining on the blank.
6, lack of mud ------ blank body incomplete phenomenon.
7. Glaze bubbles ------ Small bubbles on the surface of the glaze.
8. A series of small bubbles appear on the edge of the mouth of ------ products.
9. Billet explosion ------ Improper moisture control before the billet body enters the kiln, and local spalling caused by firing.